OK back on topic guys......
I use a product from UPOL, its essentially a copper spray,
apllied lightly and only 1-2 coats only ie almost can see through it, but dont apply any heavier or arc starting does become harder.
I have used other zinc based products that state 'weld through' and they are crap, as zinc burns off and also oxidises around the heat affected area, ie not ideal, its normally too thick even light coats does not seem to help and almost means the application is so light it does not protect anything.
The copper has no real adverse affects on any welding in thin panel steel and "in my experience" has had the best results.
Zinc sprays have problems in 1-2 years time as they seem to go salty ie oxidise a bit depending its environment and suseptability of moisture ingression.
I higly recommend the Upol product, only because of my exp with it, or any other similar products of copper type weld throguh primers.
Weld through primers are really i suppose for coating bare metal in which a resistive spot welder is used in repairs.
ie weld through not over, as the preimer is there to conduct current to keep the spot as small as possible.
HOWEVER all my experience is using a decent mig welder (wia), using a hotter than colder approach does alsways in my exp. give a flater weld with plenty of penatration, always utilising a copper backing/heatsing to keep temps down.
always peen arouns plug welds to flatten the area around the plug, this also helps in reducing the weld shrink around it. do sow whilst still red hot.
hope this helps, any q's please voice, pm me if you require a response as i may not check this topic.