Jump to content

Recommended Posts

Posted

I've just painted the radiator support area, and got an area that is 'spotty'/grainy. Just thought I would get the opinion of some pro's as to why this happened? It is the same on both sides. I went back to bare metal, etched, surface+high-build primed, then put on the black. No sanding in between (I don't think this area is that important). My guess is it is overspray from high-build that built up after spraying the vertical surface that is parallel with the radiator.

post-101596-0-69617900-1469513255_thumb.jpg

Posted

Yeah its either overspray or severe solvent-pop by laying on too many layers too fast without letting it flash off in between coats. Most likely just sprayed on dry (overspray)

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.
Note: Your post will require moderator approval before it will be visible.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...